Description
For a combination of a membrane of SrFeCo0.5Ox and an Inconel alloy, a high-temperature seal is formed between the membrane and the alloy. The seal is interposed between the alloy and the membrane, and is a fritted compound of Sr oxide and boric oxide and a fritted compound of Sr, Fe and Co oxides. The fritted compound of SrFeCo0.50Ox is present in the range of from about 30 to 70 percent by weight of the total sealant material and the fritted compound of Sr oxide and boric oxide has a mole ratio of 2 moles of the Sr oxide for each mole of boric oxide. A method of sealing a ceramic to an Inconel metal alloy is also disclosed.
Files
US5725218.pdf
Files
(387.5 kB)
| Name | Size | Download all |
|---|---|---|
|
md5:03f3f7dd59bf16c6cadd0b27324c2968
|
387.5 kB | Preview Download |
Additional details
Identifiers
- Patent application number
- US 74998096 A
- Patent number
- US 5725218 A
- Other
- oai:uchicago.tind.io:9044
Dates
- Patent filed
-
1996-11-15